Minimum local thickness
鈮40渭m
Color and color difference
The color of the coating should be the same as the standard color that the contract stipulates. aberration 鈻Eab路鈮1.5.
Indentation hardness (Print resistance)
鈮80
Adhesive force
0grade
Impact resistance
The front of the coating, after an impact test, has no phenomenon of fracture and coming off, but it is allowed to have small wrinkles in the perimeter of a concave surface.
Cup-drawing test
After a cup-drawing test with of the indentation depth of 6mm, there should not be the phenomena of splitting and coming off on the coating.
Appearance quality
The coating of a decorative surface of the powder-sprayed sectional material should be smooth and even, and it is not allowed to have such defects as flowing marks, swelling bubbles, crackles, sticking, etc, which influence the use. It is allowed to have a slight tangerine peel phenomenon, and the degree that is allowed should be indicated by a guide sample of a material object which both the supplying and demanding sides have agreed on. |